January 4, 2024
Description
Material: TPU (I used 95A - and the settings below are for this specific material) - For best results, dry your TPU (45°-65° for at least 6 hours).
Nozzle: 0.4mm
Temp: 223° C
Bed temp: (I used 0, but you can use whatever your printer manufacturer recommends)
Infill density: 10%
Infill pattern: Cross 3D
Walls: 2
Top/bottom layers: 5
Speed: 25mm/s - up to 40mm/s
Retraction: 8mm (at 45mm/s)
Fan: 20%-100%
Build plate adhesion: Skirt (glue stick encouraged)
Support: None
Bridging (Cura): On
Time: 5.5h
Material: ~32g