I printed this in ASA for strength and UV resistance and with the standard 0.4 nozzle and 0.2 Arachne layer lines. Place the flat face at the front of the model down on the build plate in order to not have to use support material. This orientation also gives the model more strength given the layer lines being built up on an angle.