GOPRINT test model explanation
Note: If the column is not straight, there is the following possibilities
1 / screw is not straight, there is a misplaced position
2 / cleaning problem
3 / Insufficient exposure, soft resin, rising deformation
Measuring the diameter of this row, refer to resin precision
If the size is small, it can be increased
If the size is large, it can be reduced.
If the vertical face is not circled, then adjust the lift speed.
Situation 1: Machine Z screw polarization value is not allowed, or the platform is uneven
Situation 2: Upper speed / lack of exposure, leading to the formation of Kongle
If there is no appearance of small characters, it is insufficient
Measuring film adhesion
The parameters of the actual model are preferably blocked by these two holes.
This row special test stacked, but if the cleaning is not in place, it will also be bonded
This has a row of detail small pits special test resin precision
GoPrint測試模型解說
注: 如柱子出現不直情况,有以下可能性
1/絲杆不直,出現錯位
2/ 清洗時碰歪了
3/暴光不足,樹脂偏軟,拉升變形
测量這排柱子的直徑可参考樹脂精度
如發現尺寸偏小, 可加层暴光
如發現尺寸偏大, 可减层暴光
假如垂直面孔不圆, 那就要调整抬升速度.
情况1: 機器Z絲杆步進值不准,或平台不平
情况2: 升速過快/暴光不足,导致孔拉变形
小字如果没有出現,那就是暴光不足
測膜粘力
打實際模型的参數最好是這兩個孔堵塞了
這排專測堆料,但假如清洗不到位,也會粘牢
這有一排細節小坑專測樹脂精度